Introduce printing common problems and solutions

1. The problem of sticky hands after printing glue

 

After the printing paste is printed and dried, there is a sticky phenomenon, which becomes more serious with the increase of temperature.

 

Reason: The main raw material of printing glue is acrylic resin, which is determined by the characteristics of the resin. If a harder resin is used, the problem of stickiness can be solved, but the adhesion force is seriously reduced. If the adhesion force is increased, a softer resin must be selected. , but the soft resin is easy to stick back.

 

Solution:

 

Use the printing glue anti-adhesive agent, add it into the printing glue and mix it evenly. After printing, the printing glue anti-adhesive agent can form a film on the surface, which does not affect the adhesion of the printing glue, and solves the problem of stickiness. question.

 

2. The solution to the phenomenon of jamming in the printing of flat screen fabrics

 

Reasons: The density of the bottom draft is not enough; the flat screen plate making operation process is improper; the quality of the printing paste is wrong.

 

Solution:

 

The manuscripts are currently produced by computer. The higher the black density, the better the shading effect of the graphic pattern of the negative. If the blackness is not enough, the shading effect will be worse, and the ultraviolet light will easily pass through, which will cause the mesh; the haze of the negative should be low. Completed, it is easy to cause excessive exposure time and cause blocking.

 

Improper development and curing process of flat screen plate making will lead to jamming. When developing, it should be taken into account that the ultraviolet light is transmitted from the printing surface of the screen to the squeegee surface, the printing surface is fully illuminated, and can be rinsed with high-pressure water; and the degree of cross-linking of the squeegee surface is smaller than that of the printing surface, and the adhesive film is not visible. When rinsing, it should be rinsed with the residual slurry of non-pressure water slurry to avoid the residual slurry from clogging the mesh. Before curing, a second exposure should be carried out to make the adhesive layer fully photosensitive and then apply the curing agent.

 

When printing, the slurry used contains impurities or undissolved particles that block the mesh, so that the color paste cannot be scraped out of the mesh during printing, so the slurry should be filtered to remove impurities before use. When making the coating adhesive, choose a good quality adhesive and a thickener with good compatibility, and the conjunctiva should not be too fast when scratching.

 

3. The process of generating pattern edges from clear to fuzzy


At the beginning of printing, because the fluidity of the paste is good, the doctor blade does not need a lot of force to cut the paste clean. With the continuous evaporation of the water in the glue, the slurry gradually thickens and the viscosity becomes larger. It is necessary to increase the particle size of the squeegee to cut off the excess slurry. Due to the increase in strength, the elastic deformation of the screen produces pattern displacement. With the disappearance of the force of the squeegee, the edge of the pattern on the screen printing surface will stick to the paste after the screen rebounds. During the second printing, These pastes migrate to the edges of the pattern, resulting in blurring of the pattern edges.

 

Solution:

 

(1) Use wire mesh with small elasticity, such as polyester mesh;

(2) Increase the tension of the wire mesh;

(3) Reduce the resilience of the wire mesh;

(4) Adjust the viscosity of the slurry at any time.

 

4. The reasons for the sharp corners of the pattern to become rounded and the loss of small dots

 

Since the slurry gradually thickens during the printing process, its fluidity becomes smaller. When passing through the mesh, the pressure of the squeegee must be increased to pass through the mesh. However, at the edge of the screen pattern, due to the cushioning effect of the photosensitive adhesive, the The squeegee cannot squeeze the slurry out of the mesh at any time, so that the slurry particles stay in the mesh to form a film, causing the mesh on the edge of the photosensitive adhesive to block.

 

Solution:

 

(1) Choose low mesh, single wire, thin wire mesh;

(2) The photosensitive glue should not be too thick;

(3) The slurry should maintain a certain fluidity at all times.

 


5. Reasons for the skinning phenomenon of the glue during the printing process

 

Any printing material has a common characteristic, that is: the thinner the ink layer, the faster the drying, and the same is true for the glue. Since the screen is larger than the pattern, there is enough space for the paste in the screen to be stacked, and it is impossible for the squeegee to clean the paste every time it is printed. Especially, a thinner ink layer is often generated above the pattern. The ink layer will form a semi-dry film in a short period of time, and these films are brought into the partial holes by the squeegee to block the mesh holes, resulting in local blockage.


Solution:

 

Use wooden strips to isolate the pattern area of ​​the screen from the screen frame to control the slurry within a certain range. The squeegee can clean the slurry on the edge of the screen pattern every time, which means that the slurry is within this range. It is impossible to produce a thin layer of ink inside, so that the phenomenon of skinning can be eliminated.

 

6. Reasons and solutions for the seepage of the paint paste prepared by yourself

 

Self-made paint pastes are water-based pastes for textile printing. Infiltration (bleeding) can be found from the following aspects.

 

(1) Synthetic fiber fabrics: such as polyester, nylon, polypropylene, etc., or blends with a high proportion of synthetic fibers. Synthetic fiber: The fabric is a hydrophobic substance, and the water-based slurry of the coating used for printing cotton fabrics is easy to permeate and smear. When printing synthetic fabrics, thick emulsified paste should be used when mixing the pulp to avoid dilution with water. If it must be diluted, it should be diluted with a thin emulsified paste. Do not dilute directly with water.

 

(2) The humidity in the air is too high, such as long-term rainy weather in the south, less or no water should be added when mixing pulp.

 

(3) Cotton fabric is a natural cellulose fiber fabric, which is a hydrophilic substance. Generally not easy to permeate. However, if the capillary effect is too high, it will also lead to osmosis. Therefore, the appropriate capillary effect is controlled at about 7-8cm. Before feeding, it is crucial to ask the manufacturer's technical indicators. If the capillary effect is too low, it will not be printed, and if the capillary effect is too high, it will cause permeation.

 

(4) Some enterprises use emulsified paste as thickener, commonly known as A-gang paste. It is emulsified with white kerosene, peregrine and synthetic dragon glue under high-speed stirring. If the A-gang pulp has quality problems and is not fully emulsified, there will be "oil circles" after printing, which will easily cause misunderstandings of "bleeding" or "watermarks". Therefore, good quality A-gang pulp should be used or a synthetic thickener should be used to overcome the occurrence of "oil ring".

 

(7) There are many comprehensive factors that cause "seepage" and "bleeding", such as the texture of the texture is too thin, too thin, and too light; the pattern area is too large; the mesh number is too low; the pressure during operation is too large; Does not correspond to the pattern, the amount of sizing is too large and so on.

 

In addition, the countertop also has a lot to do. If you use glass or plastic veneer with a very smooth hard surface, it will also cause seepage of the pallet. The outline is not clear, but should be changed to a flexible soft countertop.

coopertailor

Comments